精品在线播放-黄色av网站在线观看-五十路六十路-不卡二区-亚洲性网站-色在线看-亚洲精品9999-国产精品久久久久毛片软件-国产福利二区-欧美一级色片-91麻豆精品在线观看-亚洲午夜一区二区-噜噜啪啪-欧美a级在线-亚洲人影院

Language:CHINESESENGLISH

Home > News > Formulation process and construction technology of fireproof coating for steel structure
CONTACT US
  • Address:Pingtang Industrial District, Shipeng Village, Shishan Town, Nanhai District, Foshan City,
  • Phone:0757-81002668/0757-63323396
  • Fax:0757-81196682
  • Contact:Ben Zheng/13826981293 Kerry Lu/13751224830
  • E-mail:sbs@sbsprefabhouse.com
  • URL:http://www.qdfuda.cn

Formulation process and construction technology of fireproof coating for steel structure

Time:[2022-10-15]  Hits:2465

1. Example I of steel structure fireproof coating

20~40 portions of dodecanol fat,


50-60 parts of silica alumina mixture,


5-10 parts of titanium dioxide,


0.5~1 part of ammonium polyphosphate,


5~10 portions of trimethyl phosphate.


Features: The steel structure fire retardant coating of this process can withstand long-term high temperature baking, and has the effect of fire protection and heat insulation. It can prevent the steel from rapidly heating up in the fire and reducing its strength, and prevent the steel structure from losing its support ability and causing the collapse of the building.


2. Example II of steel structure fireproof coating


20~40 parts of water-based resin‘


50-60 parts of silica alumina mixture,


5~10 parts of titanium dioxide, 0.5~1 part of ammonium bichloride,


5~10 portions of trimethyl phosphate.


Features: The steel structure fire retardant coating of this process can withstand long-term high temperature baking, and has the effect of fire protection and heat insulation. It can prevent the steel from rapidly heating up in the fire and reducing its strength, and prevent the steel structure from losing its support ability and causing the collapse of the building.